## Pre-Processing
22
23
@@ -52,7 +53,7 @@ The ideal-plastic material can create convergence problems. These are mitigated
52
53
```
53
54
The plastic zone is marked using a two-step color scheme with the plastic proof strain of 0.2% marking the limit between the two colors. The right movie shows the longitudinal (bending) stress with color bar limits 5% above the yield limit.
54
55
55
-
<imgsrc="PE.gif"width="400"title="Plastic zone (plastic strain > 0.2%)">
56
+
<imgsrc="PE.gif"width="400"title="Plastic zone (plastic strain > 0.2%)">