Replies: 1 comment 1 reply
-
The typical one is only used to scale the variable so the solver behaves better. As long as it is within a reasonable range, its exact value should not impact the solution you get. The initial concentration is used as the initial condition of the systrem. |
Beta Was this translation helpful? Give feedback.
1 reply
Sign up for free
to join this conversation on GitHub.
Already have an account?
Sign in to comment
Uh oh!
There was an error while loading. Please reload this page.
-
In code lithium_ion_parameters there is:
Lithium plating parameters
Could you pls tell me the defference between "Initial plated lithium concentration [mol.m-3]" and "Typical plated lithium concentration [mol.m-3]"?
Why we use "Typical plated lithium concentration [mol.m-3]" as the defination of scale in lithium plating but not Initial plated lithium concentration?
Thank you so much.
Beta Was this translation helpful? Give feedback.
All reactions